OrcaSlicer Calibration Sequence and Workflow Guide

Follow OrcaSlicer's suggested calibration order, calculate max volumetric speed, compare pressure advance methods, and choose retraction settings.

The official OrcaSlicer GitHub Wiki suggests running Temperature, Max Volumetric Speed, Pressure Advance, Flow Ratio, and Retraction in that order. The walkthrough covers Temperature, Max Volumetric Speed, Pressure Advance, and Retraction.

Use the temperature tower to find a range that prints well. If several segments look good and you plan to print at higher speeds or flow rates, consider the higher end of that range.

SequenceCalibration testProfile target
FirstTemperature (nozzle)Filament temperature settings
SecondMax Volumetric SpeedFilament Max volumetric speed
ThirdPressure AdvanceFilament Pressure Advance value
FourthFlow RatioFilament Flow ratio
FifthRetractionRetraction settings

Pre-calibration checks by printer and firmware

  • Marlin firmware requires Linear Advance (M900) in firmware for the Pressure Advance tests.
  • Bambu Lab printers. Leave Flow calibration unselected when running a Pressure Advance test.
  • Extruder type. Choose the Direct Drive or Bowden Pressure Advance variant that matches your hardware. The default retraction test settings suit most direct-drive extruders. The Bowden settings below are optional starting values.

Filament calibration walkthroughs

Temperature tower

Start with nozzle temperature calibration. Nozzle temperature affects filament viscosity, which influences how well the filament flows through the nozzle and adheres to the print bed.

Print the tower, which has vertical blocks printed at different nozzle temperatures.

Evaluate each temperature segment against four checks:

  • Layer adhesion. Higher temperatures generally improve layer adhesion.
  • Stringing. Lower temperatures usually reduce stringing, but temperatures that are too low can cause it.
  • Overhangs and bridging: Check which sections bridge cleanly without sagging.
  • Surface finish. Choose a temperature that balances finish and strength at your intended print speed.

Max volumetric speed

Run Max Volumetric Speed next to find where print quality starts to degrade.

Use the prompted defaults unless you already have an idea of the lower or upper limit for your filament.

  • Start volumetric speed: 5 mm³/s (recommended default)
  • End volumetric speed: 20 mm³/s (recommended default)
  • Step increment: 0.5 per millimeter of height (recommended default)

Slice and print the generated tower. If it reaches the top without failing, print it again with a higher end volumetric speed. Inspect the walls from bottom to top for loss of gloss, the first deformation, and under-extrusion. If the material never prints glossy, look for a rougher or duller finish.

For each change you can identify, use calipers or a ruler to measure its height in millimeters from the bottom of the print. Apply the wiki formula to each height.

Volumetric Speed = start + (HeightMeasured * step)

Worked example (illustrative arithmetic using the wiki defaults):

  • Start value: 5 mm³/s
  • Step value: 0.5
  • Example height: 19 mm
  • Calculation: 5 + (19 * 0.5) = 14.5 mm³/s

Set Max volumetric speed in the filament settings a little below the calculated speed at which the walls started to deform.

Pressure advance and adaptive pressure advance

Pressure Advance compensates for extrusion pressure lag when the print head changes speed. Pick the Direct Drive or Bowden variant that matches your hardware.

On belt printers, only the Tower method is available. Pattern and Line are disabled.

PA methodHow it testsKey detail from the wiki
LinePrints lines at varying PA valuesQuick to print, but relies heavily on a good first layer (bed mesh leveling recommended)
PatternPrints a test patternAdapted from Ellis and Marlin generators
TowerIncrements PA value upward with model heightCan take longer to print and works independently of first-layer quality

For the Line method, choose the value corresponding to the most even line. For the Tower method, find the section with the best overall corners and seams. Measure its height from the bottom of the tower in millimeters. Use the tower’s start and step values to calculate Pressure Advance.

Pressure Advance = start value + (step × measured height in mm)

Save the Pressure Advance value in your filament profile.

The wiki also lists Adaptive Pressure Advance.

Retraction test

Run the retraction tower last in the core filament workflow.

Extruder setupStart lengthEnd lengthStep increment
Default (suitable for most direct-drive extruders)0 mm2 mm0.1 mm
Suggested for Bowden1 mm6 mm0.2 mm

Print the generated tower and look for the shortest retraction length that produces the cleanest section. Measure that section’s height.

Search the G-code preview for the comment Calib_Retraction_tower to confirm the exact retraction length at that height. The ordinary retract command may omit adjustments such as “Retract amount before wipe”.

For low-oozing filaments such as PLA or ABS, 0.2 mm to 0.4 mm should suffice if the tower is clean from the start. If heavy stringing persists near the top of the tower, dry the filament and check that the nozzle is installed without leaks.

Advanced printer and tolerance calibrations

The OrcaSlicer GitHub Wiki also lists advanced printer and dimensional tests, including VFA.

  • Input Shaping. Use a test tower to calibrate the firmware’s Input Shaping, or use a built-in accelerometer if your printer has one.
  • Cornering. Tunes the cornering setting selected for your firmware, including Square Corner Velocity (Klipper), Junction Deviation or Classic Jerk (Marlin, depending on configuration), and maximum instantaneous speed changes (RepRapFirmware).
  • Orca Tolerance Test: Opened in Prepare mode by right-clicking the build plate and choosing Add Handy Model. It prints a base with six hexagonal holes and a hexagon tester. The holes are assigned tolerances of 0.0 mm, 0.05 mm, 0.1 mm, 0.2 mm, 0.3 mm, and 0.4 mm. A 6 mm Allen key can also be used to check the fit. Measure the holes and the tester with calipers to adjust X-Y hole compensation and X-Y contour compensation.

Browse the OrcaSlicer Lab posts index.

Evidence and limits

This guide draws on the official OrcaSlicer GitHub Wiki pages checked on 2026-11-26. No test prints, slicer executions, or hardware measurements were performed for this page.

Sources

  1. OrcaSlicer GitHub Wiki: Calibration
  2. OrcaSlicer GitHub Wiki: Temperature Calibration
  3. OrcaSlicer GitHub Wiki: Max Volumetric Speed Calibration
  4. OrcaSlicer GitHub Wiki: Pressure Advance Calibration
  5. OrcaSlicer GitHub Wiki: Retraction Calibration
  6. OrcaSlicer GitHub Wiki: Tolerance Calibration
  7. OrcaSlicer GitHub Wiki: Input Shaping Calibration
  8. OrcaSlicer GitHub Wiki: Cornering Calibration

Related